Effect of Spheroidizing Annealing Treatment on Carbide Evolution and Impact Toughness of Vacuum‐Melted H13 Steel
Yueying Shi, Jin Yan, YaoFei Cheng, Baoguang Sang
Dalian Polytechnic University
阅读操作
确认中在文库中上传 PDF 后可生成中文音频讲解。
摘要与影响
The evolution of carbides and the impact toughness of a vacuum‐melted H13 steel were studied under different spheroidizing annealing conditions. The main carbide types identified after annealing were Cr 7 C 3 , Cr 23 C 6 , Mo 2 C, Mo 6 C, and VC. Prolonging the holding time led to a gradual increase in the average carbide size, indicating that excessively long holding times should be avoided. During isothermal holding, carbide growth followed the Ostwald ripening mechanism. The impact toughness exhibited an initial increase followed by a decrease with extended isothermal time. After 2 h of isothermal treatment, the formation of chain‐like carbides along grain boundaries resulted in lower toughness. At 3 h, these chain‐like carbides gradually dissolved, yielding carbides with moderate size and a relatively uniform distribution, corresponding to an average impact energy of 22.1 J. In contrast, further extension to 4 and 5 h promoted pronounced carbide coarsening and the dissolution of numerous fine carbides, leading to a considerable deterioration in impact toughness.
逐年被引趋势
暂无年度引用数据
关键指标
同类平均 = 1
同领域 · 同年份 · 同类型
Google Scholar 与 OpenAlex 的被引统计范围不同,数值存在差异属正常。
AI 辅助阅读
依据:摘要
可就本文提问;依据不足时会说明。
学术脉络
学科主题
材料 / 化学Metal Alloys Wear and Properties
Microstructure and Mechanical Properties of Steels · Metallurgical and Alloy Processes