Influence of apparatus geometry and deposition conditions on the structure and topography of thick sputtered coatings
John A. Thornton
阅读操作
确认中在文库中上传 PDF 后可生成中文音频讲解。
摘要与影响
Two cylindrically symmetric and complementary sputtering geometries, the post and hollow cathodes, were used to deposit thick (∼25-μ) coatings of various metals (Mo, Cr, Ti, Fe, Cu, and Al-alloy) onto glass and metallic substrates at deposition rates of 1000–2000 Å/min under various conditions of substrate temperature, argon pressure, and plasma bombardment. Coating surface topographies and fracture cross sections were examined by scanning electron microscopy. Polished cross sections were examined metallographically. Crystallographic orientations were determined by x-ray diffraction. Microstructures were generally consistent with the three-zone model proposed by Movchan and Demchishin [Fiz. Metal. Metalloved. 28, 653 (1969)]. Three differences were noted: (1) at low argon pressures a broad zone 1–zone 2 transition zone consisting of densely packed fibrous grains was identified; (2) zone 2 columnar grains tended to be faceted at elevated temperatures, although facets were often replaced by smooth flat surfaces at higher temperatures; (3) zone 3 equiaxed grains were generally not observed at the deposition conditions investigated. Hollow cathode deposition accentuated those features of coating growth that relate to intergrain shading.
逐年被引趋势
关键指标
同类平均 = 1
同领域 · 同年份 · 同类型
Google Scholar 与 OpenAlex 的被引统计范围不同,数值存在差异属正常。
AI 辅助阅读
依据:摘要
可就本文提问;依据不足时会说明。
学术脉络
学科主题
工程Metal and Thin Film Mechanics
Advanced Materials and Semiconductor Technologies · Optical Coatings and Gratings