Behavior of Precipitates in High Carbon Austenitic Heat-resisting Steels during Creep Rupture Test at 1 050°C
Kiichi NARITA, Kotaro YAMAMOTO, Kazuyo KANAMONO, Chikako HAYASHI
Kobe Steel (Japan)
阅读操作
确认中在文库中上传 PDF 后可生成中文音频讲解。
摘要与影响
A study has been made on the behavior of precipitates in niobium or titanium and niobium-containing centrifugal cast heat-resisting steels (HK40, HP and IN519) during creep rupture test at 1 050°C.(1) In the as-cast condition, iron chromium carbide of M7C3 type precipitates, except for steel IN519 (0.33%C-24%Cr-24%Ni) where M23C6 type precipitates. Titanium niobium carbonitride (MX) precipitates in the steel containing titanium and niobium, and niobium carbonitride (NbX) precipitates in the steel containing only niobium. Chromium nitride (Cr2N) precipitates except in the steel containing only niobium.(2) During creep rupture test, M7C3 in the as-cast steel changes to (Cr0.85Fe0.15)23C6. As the results of nitriding by air, Cr2N increases and complex nitride, (Cr, Fe)NbN of tetragonal lattice, precipitates in the niobium-containing steel. Moreover, substitution reaction proceeds between carbon and nitrogen or between titanium and niobium with change of lattice parameter.(3) M23C6, Cr2N and A1N are completely decomposed by hydrochloric acid (1+1) at 90°C. By the same acid M7C3, MX and NbX are decomposed gradually but (Cr, Fe) NbN is hardly decomposed.Based upon the differences in chemical stability of precipitates, the chemical composition and amount of each kind of precipitates can be successfully determined.
逐年被引趋势
暂无年度引用数据
关键指标
同类平均 = 1
同领域 · 同年份 · 同类型
Google Scholar 与 OpenAlex 的被引统计范围不同,数值存在差异属正常。
AI 辅助阅读
依据:摘要
可就本文提问;依据不足时会说明。
学术脉络
学科主题
工程High Temperature Alloys and Creep
Intermetallics and Advanced Alloy Properties · Metallurgical and Alloy Processes