Electrochemical Migration Study on Sn-58Bi Lead-Free Solder Alloy Under Dust Contamination
Fuye Lu, Han Sun, Wenlong Yang, Tianshuo Zhou, Yunpeng Wang, Haoran Ma, Haitao Ma, Jun Chen
Dalian University of Technology
阅读操作
确认中在文库中上传 PDF 后可生成中文音频讲解。
摘要与影响
With the development of electronic packaging technology toward miniaturization, integration, and high reliability, the diameter and pitch of solder joints continue to shrink. Adjacent solder joints are highly susceptible to electrochemical migration (ECM) due to the synergistic effects of high-density electric fields, water vapor, and contaminants. Dust has become one of the non-negligible causal factors in ECM studies due to air pollution. In this study, 0.2 mM/L NaCl and Na2SO4 solutions were used to simulate soluble salt in dust, and the failure mechanism of an Sn-58Bi solder ECM in the soluble salt in dust was analyzed by a water-droplet experimental method. It was shown that the mean failure time of the ECM of an Sn-58Bi solder in an NaCl solution (53 s) was longer than that in an Na2SO4 solution (32 s) due to the difference in the anodic dissolution characteristics in the two soluble salt solutions. XPS analysis revealed that the dendrites produced by the ECM process were mainly composed of Sn, SnO, and SnO2, and there were precipitation products—Sn(OH)2 and Na2SO4—attached to the dendrites. The corrosion potential in the NaCl solution (−0.351 V) was higher than that in the Na2SO4 solution (−0.360 V), as shown by a polarization test, indicating that the Sn-58Bi solder had better corrosion resistance in the NaCl solution. Therefore, an Sn-58Bi solder has better resistance to electrochemical migration in an NaCl solution compared to an Na2SO4 solution.
逐年被引趋势
关键指标
同类平均 = 1
同领域 · 同年份 · 同类型
Google Scholar 与 OpenAlex 的被引统计范围不同,数值存在差异属正常。
AI 辅助阅读
依据:摘要
可就本文提问;依据不足时会说明。
学术脉络
学科主题
工程Electronic Packaging and Soldering Technologies
Corrosion Behavior and Inhibition · Electrodeposition and Electroless Coatings